Roda Potong A60 (Amat Keras)
Penerangan: Bahan Aluminium Oksida,Ikatan Resin.
Permohonan: Untuk memotong logam ferus yang sangat keras (HRC>55).
| Pesanan No | Kod | Spesifikasi (mm) | Pakej |
| 01.01.111 | A601505 | 150*12.7*0.5 | 10 pcs |
| 01.01.114-1 | A601808 | 180*12.7*0.8 | 10 pcs |
| 01.01.118 | A602008 | 200*22.0*0.8 | 10 pcs |
| 01.01.150 | A602515 | 250*32.0*1.5 | 10 pcs |
| 01.01.160 | A603020 | 300*32.0*2.0 | 10 pcs |
| 01.01.170 | A603525 | 350*32.0*2.5 | 10 pcs |
| 01.01.180 | A604030 | 400*32.0*3.0 | 10 pcs |
| 01.01.185 | A604530 | 450*32.0*3.2 | 10 pcs |
| 01.01.190 | A605040 | 508*50.8*4.0 | 10 pcs |
A 50 Potongan Roda(Sederhana Keras)
Penerangan: Bahan Aluminium Oksida,Ikatan Resin.
Permohonan: Untuk memotong logam ferus sederhana keras (HRC40-55).
| Pesanan No | Kod | Spesifikasi (mm) | Pakej |
| 01.01.213-1 | A501505 | 150*12.7*0.5 | 10 pcs |
| 01.01.214 | A501808 | 180*12.7*0.8 | 10 pcs |
| 01.01.224 | A502008 | 200*22.0*0.8 | 10 pcs |
| 01.01.250 | A502515 | 250*32.0*1.5 | 10 pcs |
| 01.01.260 | A503020 | 300*32.0*2.0 | 10 pcs |
| 01.01.270 | A503525 | 350*32.0*2.5 | 10 pcs |
| 01.01.280 | A504030 | 400*32.0*3.0 | 10 pcs |
| 01.01.285 | A504530 | 450*32.0*3.2 | 10 pcs |
| 01.01.290 | A505040 | 508*50.8*4.0 | 10 pcs |
A 30 Potongan Roda(Lembut)
Penerangan: Bahan Aluminium Oksida,Ikatan Resin.
Permohonan: Untuk memotong logam ferus lembut (HRC20-40).
| Pesanan No | Kod | Spesifikasi (mm) | Pakej |
| 01.01.313 | A301505 | 150*12.7*0.5 | 10 pcs |
| 01.01.314 | A301808 | 180*12.7*0.8 | 10 pcs |
| 01.01.315 | A302008 | 200*22.0*0.8 | 10 pcs |
| 01.01.350 | A302515 | 250*32.0*1.5 | 10 pcs |
| 01.01.360 | A303020 | 300*32.0*2.0 | 10 pcs |
| 01.01.370 | A303525 | 350*32.0*2.5 | 10 pcs |
| 01.01.380 | A304030 | 400*32.0*3.0 | 10 pcs |
| 01.01.385 | A304530 | 450*32.0*3.2 | 10 pcs |
| 01.01.390 | A305040 | 508*50.8*4.0 | 10 pcs |
Roda Potong S20(Lembut Bukan Ferus)
Penerangan: Bahan Silicon Carbide,Resin Bond.
Permohonan: Untuk memotong Aloi Non-Ferus,AI, Cu yang lembut.
| Pesanan No | Kod | Spesifikasi (mm) | Pakej |
| 01.02.413 | S201505 | 150*25.4*0.5 | 10 pcs |
| 01.02.422 | S202008 | 200*22.0*0.8 | 10 pcs |
| 01.02.450 | S202515 | 250*32.0*1.5 | 10 pcs |
| 01.02.460 | S203020 | 300*32.0*2.0 | 10 pcs |
| 01.02.470 | S203525 | 350*32.0*2.5 | 10 pcs |
| 01.02.480 | S204030 | 400*32.0*3.0 | 10 pcs |
| 01.02.485 | S204530 | 450*32.0*3.2 | 10 pcs |
| 01.02.490 | S205040 | 508*50.8*4.0 | 10 pcs |
Produk Serupa
| Trojan | Struers | Buehler | ATM |
| A60 ** ** | 60A** | Bahan ferus>HRC 60 | Siri C |
| A50 ** ** | 50A** | Bahan ferus HRC 50- 60 | Siri D |
| A30 ** ** | 30A** | Bahan ferus HRC 35-50 | Siri E |
| S20 *** | 20A** | Bahan mulur | Siri F |
| A60 20 08 | 60A20 | Bahan ferus>HRC 60 | Siri C |
| A30 20 08 | 30A20 | Bahan ferus HRC 35-50 | Siri E |
| A50 25 15 | 50A25 | Bahan ferus HRC 50- 60 | Siri D |
| S20 25 15 | 20S25 | Bahan mulur | Siri F |
| A60 30 20 | 60A30 | Bahan ferus>HRC 60 | Siri C |
| A30 30 20 | 30A30 | Bahan ferus HRC 35-50 | Siri E |
| A50 40 30 | 50A40 | Bahan ferus HRC 50- 60 | Siri D |
| S20 40 30 | 20S40 | Bahan mulur | Siri F |
| A60 50 40 | 60A50 | Bahan ferus>HRC 60 | Siri C |
| A30 50 40 | 30A50 | Bahan ferus HRC 35-50 | Siri E |